Titanium in Nitric Acid: Rates, the Mid-Range Peak, and the Hard Limits
In boiling 90 percent nitric acid on a heating surface, the tests published by TIMET put unalloyed titanium at 1.0 to 6.6 mpy (0.03 to 0.17 mm/y) while Type 304L stainless ran 150 to 2,900 mpy (3.8 to 73.7 mm/y) in the same TIMET tests. That two-to-three order of magnitude gap is why nitric acid